Material: |
99% Alumina Ceramic |
Color: |
Light Yellow |
Density: |
3.9g/cm³ |
Working Temperature: |
1700℃ |
OEM,ODM: |
Acceptable |
Origin: |
China |
MOQ: |
100 Pcs |
Package: |
Carton |
Size: |
Customized |
Material: |
99% Alumina Ceramic |
Color: |
Light Yellow |
Density: |
3.9g/cm³ |
Working Temperature: |
1700℃ |
OEM,ODM: |
Acceptable |
Origin: |
China |
MOQ: |
100 Pcs |
Package: |
Carton |
Size: |
Customized |
Industrial ceramic precision polishing 99% Alumina ceramic rod
Alumina ceramic is a kind of structural ceramics, with insulation resistance, voltage resistance, high strength, good thermal conductivity, dielectric loss, stable electrical performance characteristics. Used in electronic ceramic substrates, ceramic electrical insulation, vacuum devices, devices porcelain, spark plugs and other products.
Alumina rod is made of aluminum oxide (Al2O3) ceramic – a fine ceramic material that is widely used in various industries. Aluminum oxide rod has superb performance in electrical insulation, high chemical resistance, and low thermal expansion.According to actual application and customer's requirement, the purities vary from 95%-99.7% and the forming methods will be different. The forming methods applied in our plant include dry pressing, isostatic pressing, injection moulding, extrusion moulding. With experienced engineers and talented workers, we are confident to offer high quality, high precision, complex components for customers worldwide.
Properties | Unit | Steatite ceramic | 95% Al2O3 | 99% Al2O3 | Zirconia Ceramic |
Density | g/cm³ | 2.8 | 3.6 | 3.8 | 5.6 |
Flexural strength | Mpa | 145 | 300 | 300 | 354 |
Max Working Temperature | ℃ | 1100 | 1400 | 1600 | 1400 |
Sintering temperature | ℃ | 1350 | 1700 | 1750 | 1550 |
Heat resistance | T(℃) | 200 | 220 | 200 | 350 |
Hardness | Gpa | 5.7 | 7 | 10.7 | 12.3 |
Elastic modulus | Gpa | 120 | 275 | 320 | 205 |
Poissons ratio | - | 0.21 | 0.22 | 0.22 | 0.30 |
Linear expansion coefficient | x 10-6/℃ | 7.9 | 7.1 | 7.8 | 9 |
Insulation breakdown Intensity | KT/mm | 10 | 16 | 18 | 15 |
Thermal conductivity | w/(m.k) | 2.5 | 20 | 25 | 2.5 |
Specific Heat | *10-3J/(kg*K) | 0.75 | 0.78 | 0.78 | 0.4 |